Study on Formability of 3D Porous Scaffolds Prepared by DNA / Chitosan
DNA/幾丁聚醣製備3D多孔支架之成形性研究
X. Y. Chen1, C. P. Chang2
陳宣宇1,張志鵬2
In this study, 3D porous scaffolds were prepared with fixed DNA concentration of 5% and chitosan at different concentrations of 1%, 2% and 3%. Porosity will be with the speed and chitosan concentration increased and smaller, porosity can be maintained at 80% or more. 3D porous Scaffolds will increase with the chitosan concentration, the formability will better.
本研究是以固定去氧核醣核酸(DNA)濃度為5%以及不同濃度幾丁聚醣(Chitosan)分別為1%、2%、3%製成3D多孔支架,利用傅立葉可見光吸收光譜儀得知皆含有DNA以及幾丁聚醣之特定官能基。3D多孔支架的孔徑大小會隨著均質機轉速的增加而有所減少,孔隙率會隨著轉速與幾丁聚醣濃度的提高而越來越小,孔隙率都能維持在80%以上,3D多孔支架會隨著幾丁聚醣濃度增加,成形性越佳。
DNA, Chitosan, 3D Porous Scaffolds, Porosity
去氧核醣核酸, 幾丁聚醣, 3D多孔支架, 孔隙率
Year Volume
2020 27.1 | 27.2
27.3 |
2019 26.1 |
2018 25.1 |
2017 24.1 | 24.2
24.3 | 24.4
24.5 | 24.6
24.7 | 24.8
24.9 |
2016 23.1 | 23.2
23.3 | 23.4
23.5 | 23.6
23.7 | 23.8
2015 22.1 | 22.2
22.3 | 22.4
22.5 |
2014 21.1 | 21.2
21.3 |
2013 20.1 | 20.2
20.3 | 20.4
2012 19.1 | 19.2
19.3 | 19.4
2011 18.1 | 18.2
2010 17.4